GB/T 3810.13-2016 is a test method for evaluating the resistance of ceramic tile surfaces to chemical reagent erosion. It exposes tile samples to various chemical agents commonly found in household and industrial environments, such as acids, alkalis, salt solutions, swimming pool chlorides, etc. By observing whether visible physical or chemical changes occur on the surface, the chemical corrosion resistance grade is assessed. This is particularly important for tiles used in special environments such as laboratories, chemical plants, and swimming pools.
This summary is not the original standard text and is for reference only. For accurate information, please obtain it through official channels.
| Status | Active | ||
|---|---|---|---|
| CCS | Q31 | ICS | 91.100.25 |
| Release Date | 2016-04-25 00:00:00 | Implementation Date | 2017-03-01 00:00:00 |