GB/T 26930.6-2014 "Carbonaceous materials used in the production of aluminium - Coal tar pitch - Part 6: Determination of ash content" specifies the method for determining the ash content of coal tar pitch used in the production of primary aluminium. The method employs a high-temperature incineration process, in which a specified mass of coal tar pitch sample is gradually heated to a specific high temperature in a muffle furnace under defined conditions and incinerated to constant weight. The percentage of the residue's mass relative to the original sample's mass represents the ash content.
This summary is not the original standard text and is for reference only. For accurate information, please obtain it through official channels.